Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3K FC Aqua UN - PA66 - BASF

Material Data Center offers the following functions for Ultramid® A3K FC Aqua UN:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Ultramid® A3K FC Aqua UN is optimized for plastic parts, mandatory requiring material approvals for drinking water or direct food contact.

The product is approved according to
• 21 CFR FDA § 177.1500 "Nylon resins" (except contact with alcoholic beverages)
• European Food Contact European Food Contact Commission Regulation (EU) 10/2011
• GMP (EC) n°2023/2006

and provides the approvals for drinking water regulations of
• KTW
• DVGW W270
• WRAS
• ACS (disclosure of ingredients)
• NSF (disclosure of ingredients)

For questions regarding the compliance with further regulations, and certificates, please contact your local BASF representative or Plastics Safety (E-Mail: plastics.safety@basf.com).
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 115 / * cm³/10min ISO 1133
Température 275 / * °C -
Charge 5 / * kg -
Retrait au moulage, parallèle 1.6 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.8 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 3100 / 1100 MPa ISO 527
Contrainte d'écoulement 85 / 50 MPa ISO 527
Déformation au seuil d'écoulement 5 / 20 % ISO 527
Déformation nominale à la rupture 30 / >50 % ISO 527
Module de flexion, 23°C 2900 / - MPa ISO 178
Module de fluage en traction, 1h * / 1100 MPa ISO 899-1
Module de fluage en traction, 1000h * / 700 MPa ISO 899-1
Résistance au choc Charpy, +23°C N / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 5 / 20 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 4 / - kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille, +23°C 5.5 / N kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 6 / - kJ/m² ISO 180/1A
Température -30 °C -
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 260 / * °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 72 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 75 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 220 / * °C ISO 75-1/-2
Température de ramolliss. Vicat, B 250 / * °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 98 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-2 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Aptitude à l'allumage 28 / * % ISO 4589-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.8 / - - IEC 62631-2-1
Permittivité relative, 1MHz 3.2 / 5 - IEC 62631-2-1
Facteur de pertes, 100Hz 50 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 250 / 2000 E-4 IEC 62631-2-1
Résistivité transversale 1E13 / 1E10 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 1E10 Ohm IEC 62631-3-2
Indice de résistance au cheminement - / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 8.5 / * % Sim. to ISO 62
Absorption d'humidité 2.8 / * % Sim. to ISO 62
Masse volumique 1130 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
Propriétés spécifiques à la matièresec / condUnitéNorme du test
ISO Data
Indice de viscosité 150 / * cm³/g ISO 307, 1157, 1628
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 4 h -
L'humidité de traitement ≤0.15 % -
Température de la matière fondue 280 - 300 °C -
Température du moule 60 - 80 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Ultramid® A3K FC Aqua UN, PA66, BASF
Contrainte de cisaillement / Vit. de cisaillement , Ultramid® A3K FC Aqua UN, PA66, BASF
Module de cisaillement dynamique / Température , Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Module de cisaillement dynamique / Température , Ultramid® A3K FC Aqua UN (cond.), PA66, BASF
Contrainte / Déformation , Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Contrainte / Déformation , Ultramid® A3K FC Aqua UN (cond.), PA66, BASF
Module sécant / Déformation , Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Module sécant / Déformation , Ultramid® A3K FC Aqua UN (cond.), PA66, BASF
Contrainte / Déformation (isochrone) 23°C, Ultramid® A3K FC Aqua UN (cond.), PA66, BASF
Module de fluage / Temps 23°C, Ultramid® A3K FC Aqua UN (cond.), PA66, BASF
Courbe de fluage 23°C, Ultramid® A3K FC Aqua UN (cond.), PA66, BASF
Contrainte / Déformation (isochrone) 60°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Module de fluage / Temps 60°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Courbe de fluage 60°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Contrainte / Déformation (isochrone) 90°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Module de fluage / Temps 90°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Courbe de fluage 90°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Contrainte / Déformation (isochrone) 120°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Module de fluage / Temps 120°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Courbe de fluage 120°C, Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Volume spécifique (pvT) , Ultramid® A3K FC Aqua UN, PA66, BASF
Module de traction / Température , Ultramid® A3K FC Aqua UN (sec), PA66, BASF
Module de traction / Température , Ultramid® A3K FC Aqua UN (cond.), PA66, BASF
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant, Agent de démoulage
Propriétés spéciales
Stabilisé à la chaleur
Certifications
Contact alimentaire, Approuvé pour le contact alimentaire suivant 10/2011, FDA 21 CFR approbation, Contact avec l'eau potable, Contact avec l'eau potable KTW, Contact avec l'eau potable DVGW W270, Contact avec l'eau potable NSF 61
Applications
Automobile
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 60 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.